Advanced Polymer Alloys DuraGrip™ DGR 6160 NC Thermoplastic Elastomer (TPE)

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer APA - Advanced Polymer Alloys
Trade Name DuraGrip™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Advanced Polymer Alloys DuraGrip™ DGR 6160 NC Thermoplastic Elastomer (TPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuraGrip® DGR 6160 is offered in an NC (colorable) version, and is designed to chemically bond to a wide variety of thermoplastic substrates including ABS, PC, Nylon 6, Nylon 6/6, glass filled Nylon, ASA, PC/ABS alloys, PBT, and PC/PBT alloys. It is easy to use in injection molding and extrusion processes. DGR 6160NC has excellent elastomeric properties and soft touch feel. DuraGrip® bonding grades are hygroscopic, and for best results drying is recommended prior to use.Information provided by Advanced Polymer Alloys
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D471
Viscosity 354000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
354000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
5 Sec; ASTM D2240
Tensile Strength at Break 6.60 MPa
957 psi
ASTM D412
Elongation at Break 350 %
350 %
ASTM D412
100% Modulus 0.00220 GPa
0.319 ksi
ASTM D412
Graves Tear Strength 34.9 kN/m

@Temperature 24.0 °C
199 pli

@Temperature 75.2 °F
Die C; ASTM D624
Compression Set 21 %
21 %
after 22 Hr At 24°C; ASTM D395
Tensile Set 4.0 %
4.0 %
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -65.0 °C
-85.0 °F
ASTM D746
Descriptive Properties Value Comments
Color N,B