Adell RA-18 Copolymer Polypropylene, 40% Talc Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Talc Filler
Manufacturer Adell Plastics, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell RA-18 Copolymer Polypropylene, 40% Talc Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.235 g/cc
0.04462 lb/in³
ASTM D792
Water Absorption 0.040 %
0.040 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 50
50
ASTM D785
Hardness, Rockwell R 79
79
ASTM D785
Tensile Strength, Ultimate 25.5 MPa
3700 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Strength 35.9 MPa
5210 psi
ASTM D790
Flexural Modulus 2.10 GPa
305 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.90 J/cm
5.43 ft-lb/in
ASTM D256
Gardner Impact 1.10 J
0.811 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 132 °C
270 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ASTM D648
Flammability, UL94 HB
HB