Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Addiplast Addilene J 370 Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Addiplast
Trade Name Addilene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addiplast Addilene J 370 Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High impact strength, high elongation at breakInformation provided by Addiplast.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183/A
Melt Flow 5.0 g/10 min
5.0 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ISO 868
Tensile Strength at Break 18.0 MPa
2610 psi
ISO R 527
Tensile Strength, Yield 22.0 MPa
3190 psi
ISO R 527
Elongation at Yield >= 500 %
>= 500 %
ISO R 527
Modulus of Elasticity 0.950 GPa
138 ksi
ISO 178
Izod Impact, Notched (ISO) NB
NB
ISO 180/1A
Charpy Impact Unnotched NB
NB
ISO 179/IeU
Charpy Impact, Notched 4.00 J/cm²
19.0 ft-lb/in²
ISO 179/IeA
Thermal Properties Metric English Comments
Melting Point 165 - 168 °C
329 - 334 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C
118 °F
ISO 75-2/AF
Vicat Softening Point 141 °C
286 °F
ISO 306/A50
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
CEI 60093
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
CEI 60093
Comparative Tracking Index >= 600 V
>= 600 V
CEI 60112/Solution A
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved