Material Notes:
Fields of application: Functionalised polypropylene to be used as compatibiliser for polymer blends or coupling agent for glass fiber, wood flour, natural fibers, multilayer films, aluminum foils, or mineral filled polypropylene.Examples: Compatibilising short-and long glass fibers and PP applications such as automotive applications (instrument panel carrier, front-end, door modules, etc.) and Wood filled polymer composites.Mode of action and advantages: PRIEX® 25097 is a polypropylene, grafted with a very high content of maleic anhydride. The grafted maleic anhydride introduces polarity to the polymer achieving compatibility between polyolefins and more polar polymers like EVOH.Advantages: Excellent mechanical properties, good cost / performance; Ultra low smell, low VOC and emissions; Lower melting point compared to similar PP homopolymer PRIEX® grades; Excellent wetting properties as a result of very low viscosity (hyperfluid grade); Excellent coupling agent for short and long glass filled polyolefins providing enhanced physical, mechanical and thermal properties; Excellent coupling agent for natural fiber reinforced polymer composites or wood flour reinforced polymer composites; Free flowing pellets; and Safe and easy handling.Food contact: PRIEX® 25093 composition meets the requirements of Commission Directive 2002/72/EC and further amendments.Information provided by Addcomp Polymer Additive Solutions
Physical Properties Metric English Comments
Oxidative Induction Time (OIT) 40 min

@Temperature 190 °C
40 min

@Temperature 374 °F
ISO 11357-6
Melt Flow 15 - 20 g/10 min

@Load 1.20 kg,
Temperature 190 °C
15 - 20 g/10 min

@Load 2.65 lb,
Temperature 374 °F
die 8/1; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.0 MPa
2470 psi
ISO 527-2
Elongation at Break 3.1 %
3.1 %
ISO 527-2
Modulus of Elasticity 0.717 GPa
104 ksi
1 mm/min; ISO 527-1
Thermal Properties Metric English Comments
Melting Point 135 - 145 °C
275 - 293 °F
ISO 11357-3
Crystallization Temperature 90.0 °C
194 °F
ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °C
162 °F
ISO 75
Processing Properties Metric English Comments
Processing Temperature <= 280 °C
<= 536 °F
Descriptive Properties Value Comments
Appearance White or slightly yellow granules
Free Aleic Anhydride <50 mg/kg
Solvay method
Grafted Maleic Anhydride 0.45-0.48%
Solvay method
Copyright © lookpolymers.com All Rights Reserved