Addcomp ADD-VANCE® SA 420 Slip/anti-block additive

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Addcomp
Trade Name ADD-VANCE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addcomp ADD-VANCE® SA 420 Slip/anti-block additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fields of application: Improves slip and anti-block properties of thermoplastics. It can also be used as a release agent for injection molded products.Examples: (L)LDPE, HDPE, PP, PS, HIPS, TPO, ABS and other thermoplastics which are processed in films, sheets, profiles, injection molded products, etc.Mode of action and advantages: ADD-VANCE SA 420 provides slip and anti-block properties. ADD-VANCE SA 420 reduces friction between two surfaces for instance between polymer and metal. As a consequence the slip properties of the product are improvedAdvantages: Excellent anti-block properties, already at low dosing rates; Excellent organoleptic properties; Good printability; Non-toxic and non-corrosive; Injection molding: also improved demoulding and product release; Non-sticking pellets, dust free dosing; and Safe and easy handlingRegulations: ADD-VANCE SA 420 is suitable for food packaging products as the active ingredients are in compliance with current food contact regulations.Information provided by ADDCOMP
Processing Properties Metric English Comments
Processing Temperature <= 220 °C
<= 428 °F
Descriptive Properties Value Comments
Appearance White to off-white granules
Dosing Level 0.3-1%