Addcomp ADD-VANCE® BA 131 Blowing agent

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Addcomp
Trade Name ADD-VANCE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addcomp ADD-VANCE® BA 131 Blowing agent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fields of application: Foamed products of polyolefins and other polymers. Extruded sheets and foams in general as well as injection moulded parts that require a foamed core.Mode of action and advantages: ADD-VANCE® BA 131 contains a proprietary combination of endothermic blowing agent additives. ADD-VANCE® BA 131 contains a very high level of active components and NO polymer carrier.Advantages: Universal blowing agent for polyolefins and other polymers (e.g. polyamide); Excellent foam development and fine cell structure; Cost savings due to reduced polymer use; Weight reduction of the final part; Cost efficient: the product is very effective at low dosing rates: 0.5 – 1.0 wt%; Foam densities of 0.5 – 0.6 g / dm3 have been achieved in polyolefins during in house laboratory evaluations; and Easy to use.Regulations: ADD-VANCE® BA 131 is suitable for food packaging products as the active ingredients are in compliance with current food contact regulationsInformation provided by ADDCOMP
Processing Properties Metric English Comments
Processing Temperature <= 300 °C
<= 572 °F
Descriptive Properties Value Comments
Appearance White granules
Dosing Level 0.5-1%
Foam densities 0.5-0.6 g/dm3