Material Notes:
Information provided by Adamas, HPM
Physical Properties Metric English Comments
Specific Gravity 2.15 - 2.17 g/cc
2.15 - 2.17 g/cc
ASTM D792
Water Absorption 0.015 %
0.015 %
ASTM D570
Deformation 6.0 - 6.9 %
6.0 - 6.9 %
Permanent deformation after 24 hrs @ 23°C; ASTM D621
10 - 12.9 %
10 - 12.9 %
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 52 - 56
52 - 56
ASTM D2240
Ball Indentation Hardness 40.0 - 46.0 MPa
5800 - 6670 psi
ISO 2032-N132
Tensile Strength at Break >= 26.0 MPa
>= 3770 psi
ASTM D4745-11
Elongation at Break >= 240 %
>= 240 %
ASTM D4745-11
Coefficient of Friction, Dynamic 0.060 - 0.080
0.060 - 0.080
ASTM D1894
Coefficient of Friction, Static 0.016 - 0.60
0.016 - 0.60
ASTM D1894
Thermal Properties Metric English Comments
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C 177
Melting Point 327 °C
621 °F
DSC
Maximum Service Temperature, Air 260 °C
500 °F
DSC
Minimum Service Temperature, Air -80.0 °C
-112 °F
DSC
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+8 ohm-cm
1.00e+8 ohm-cm
ASTM D257
Surface Resistance 1.00e+6 ohm
1.00e+6 ohm
ASTM D257