Material Notes:
Information provided by Adamas, HPM
Physical Properties Metric English Comments
Specific Gravity 1.90 - 1.93 g/cc
1.90 - 1.93 g/cc
ASTM D792
Deformation 4.0 - 10 %
4.0 - 10 %
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 57 - 62
57 - 62
ASTM D2240
Tensile Strength at Break >= 15.0 MPa
>= 2180 psi
ASTM D4745-97
Elongation at Break >= 160 %
>= 160 %
ASTM D4745-97
Coefficient of Friction, Dynamic 0.18 - 0.22
0.18 - 0.22
ASTM D1894
Coefficient of Friction, Static 0.25 - 0.45
0.25 - 0.45
ASTM D1894
Thermal Properties Metric English Comments
Thermal Conductivity 0.370 W/m-K
2.57 BTU-in/hr-ft²-°F
ASTM C 177
Melting Point 327 °C
621 °F
DSC
Maximum Service Temperature, Air 250 °C
482 °F
DSC
Minimum Service Temperature, Air -85.0 °C
-121 °F
DSC
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
ASTM D257
Dielectric Constant 1.9

@Frequency 60.0 - 2.00e+6 Hz
1.9

@Frequency 60.0 - 2.00e+6 Hz
ASTM D150
Dielectric Strength 20.0 - 50.0 kV/mm
508 - 1270 kV/in
ASTM D149