Adamas Adalon® 139 PTFE, 35% Soft Carbon Filled

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Carbon Fiber Filled
Manufacturer Adamas
Trade Name Adalon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adamas Adalon® 139 PTFE, 35% Soft Carbon Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Adamas, HPM
Physical Properties Metric English Comments
Specific Gravity 2.04 - 2.08 g/cc
2.04 - 2.08 g/cc
ASTM D792
Deformation 2.0 - 3.1 %
2.0 - 3.1 %
Permanent deformation after 24 hrs @ 23°C; ASTM D621
4.5 - 5.4 %
4.5 - 5.4 %
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 62 - 64
62 - 64
ASTM D2240
Tensile Strength at Break >= 15.0 MPa
>= 2180 psi
ASTM D4894
Elongation at Break >= 40 %
>= 40 %
ASTM D4894
Coefficient of Friction, Dynamic 0.13 - 0.15
0.13 - 0.15
ASTM D1894
Coefficient of Friction, Static 0.14 - 0.16
0.14 - 0.16
ASTM D1894
Thermal Properties Metric English Comments
Thermal Conductivity 0.290 W/m-K
2.01 BTU-in/hr-ft²-°F
ASTM C 177
Melting Point 327 °C
621 °F
DSC
Maximum Service Temperature, Air 260 °C
500 °F
DSC
Minimum Service Temperature, Air -80.0 °C
-112 °F
DSC
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
ASTM D257
Surface Resistance 1000 ohm
1000 ohm
ASTM D257