Aclo Accutech Polypropylene HP0335G30CHIV Homopolymer Glass Reinforced High Impact Coupled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Glass Reinforced, Impact Modified
Manufacturer Aclo Compounders
Trade Name Accutech
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene HP0335G30CHIV Homopolymer Glass Reinforced High Impact Coupled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Approved to GMP.PP.017 Black A12563
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Melt Flow 4.0 g/10 min
4.0 g/10 min
ASTM D1238
Ash 27 - 33 %
27 - 33 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 77.01 MPa
11170 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Tensile Modulus 4.499 GPa
652.5 ksi
ASTM D638
Flexural Strength 80.0 MPa
11600 psi
ASTM D790
Flexural Modulus 4.699 GPa
681.5 ksi
ASTM D790
Izod Impact, Notched 1.01 J/cm
1.90 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 155 °C
311 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 140 °C
284 °F