Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aclo Accutech Polypropylene Copolymer CP0437T10L Talc Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Talc Filler
Manufacturer Aclo Compounders
Trade Name Accutech
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Copolymer CP0437T10L Talc Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
MD; ASTM D955
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Ash 10 %
10 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 66
66
ASTM D785
Tensile Strength at Break 13.0 MPa
1890 psi
ASTM D638
Tensile Strength, Yield 17.0 MPa
2470 psi
ASTM D638
Elongation at Break 45 %
45 %
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Tensile Modulus 1.00 GPa
145 ksi
ASTM D638
Flexural Strength 20.0 MPa
2900 psi
ASTM D790
Flexural Modulus 1.100 GPa
159.5 ksi
ASTM D790
Izod Impact, Notched 1.44 J/cm
2.70 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.2 °C
180 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 52.2 °C
126 °F