Aclo Accutech Polypropylene Copolymer CP0437G20M10CL Glass/Mineral Reinforced Coupled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Glass/Mineral Reinforced
Manufacturer Aclo Compounders
Trade Name Accutech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Copolymer CP0437G20M10CL Glass/Mineral Reinforced Coupled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
MD; ASTM D955
Melt Flow 9.0 g/10 min
9.0 g/10 min
ASTM D1238
Ash 30 %
30 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 69
69
ASTM D785
Tensile Strength at Break 35.0 MPa
5080 psi
ASTM D638
Tensile Strength, Yield 37.0 MPa
5370 psi
ASTM D638
Elongation at Break 9.0 %
9.0 %
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Tensile Modulus 2.899 GPa
420.5 ksi
ASTM D638
Flexural Strength 52.0 MPa
7540 psi
ASTM D790
Flexural Modulus 3.20 GPa
464 ksi
ASTM D790
Izod Impact, Notched 1.55 J/cm
2.90 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 152 °C
306 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
248 °F
Users viewing this material also viewed the following: