Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aclo Accutech Polypropylene Copolymer CP0436T10L1 Talc Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Talc Filler
Manufacturer Aclo Compounders
Trade Name Accutech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Copolymer CP0436T10L1 Talc Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
Linear Mold Shrinkage 0.011 cm/cm
0.011 in/in
MD; ASTM D955
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Ash 10 %
10 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 63
63
ASTM D785
Tensile Strength at Break 17.0 MPa
2470 psi
ASTM D638
Tensile Strength, Yield 23.0 MPa
3340 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Tensile Modulus 1.40 GPa
203 ksi
ASTM D638
Flexural Strength 29.0 MPa
4210 psi
ASTM D790
Flexural Modulus 1.40 GPa
203 ksi
ASTM D790
Izod Impact, Notched 1.01 J/cm
1.90 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 52.8 °C
127 °F