Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aclo Accutech Polypropylene Copolymer CP0436M40L Mica Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Mica Filler
Manufacturer Aclo Compounders
Trade Name Accutech
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Copolymer CP0436M40L Mica Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
MD; ASTM D955
Melt Flow 7.0 g/10 min
7.0 g/10 min
ASTM D1238
Ash 40 %
40 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 42
42
ASTM D785
Tensile Strength at Break 21.0 MPa
3050 psi
ASTM D638
Tensile Strength, Yield 22.0 MPa
3190 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Elongation at Yield 2.0 %
2.0 %
ASTM D638
Tensile Modulus 3.40 GPa
493 ksi
ASTM D638
Flexural Strength 31.0 MPa
4500 psi
ASTM D790
Flexural Modulus 4.400 GPa
638.1 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 123 °C
253 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 72.8 °C
163 °F