Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
Manufacturer Aclo Compounders
Trade Name Accutech
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Copolymer CP0436C40L1 Calcium Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
MD; ASTM D955
Melt Flow 9.0 g/10 min
9.0 g/10 min
ASTM D1238
Ash 40 %
40 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 58
58
ASTM D785
Tensile Strength at Break 15.0 MPa
2180 psi
ASTM D638
Tensile Strength, Yield 18.0 MPa
2610 psi
ASTM D638
Elongation at Break 35 %
35 %
ASTM D638
Elongation at Yield 2.0 %
2.0 %
ASTM D638
Tensile Modulus 1.900 GPa
275.5 ksi
ASTM D638
Flexural Strength 25.0 MPa
3630 psi
ASTM D790
Flexural Modulus 1.60 GPa
232 ksi
ASTM D790
Izod Impact, Notched 1.28 J/cm
2.40 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 53.9 °C
129 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 93.9 °C
201 °F