Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aclo Accutech Polyethylene HD0204UVL High Density UV Stabilized

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Aclo Compounders
Trade Name Accutech
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polyethylene HD0204UVL High Density UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ASTM D792
Linear Mold Shrinkage 0.018 cm/cm
0.018 in/in
MD; ASTM D955
Melt Flow 7.0 g/10 min
7.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 50
50
ASTM D785
Tensile Strength at Break 14.0 MPa
2030 psi
ASTM D638
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Tensile Modulus 1.00 GPa
145 ksi
ASTM D638
Flexural Strength 21.0 MPa
3050 psi
ASTM D790
Flexural Modulus 0.800 GPa
116 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.8 °C
190 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C
113 °F
Users viewing this material also viewed the following: