Material Notes:
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Melt Flow 7.0 g/10 min
7.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.8 MPa
3600 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Tensile Modulus 1.80 GPa
261 ksi
ASTM D638
Flexural Strength 65.0 MPa
9430 psi
ASTM D790
Flexural Modulus 2.099 GPa
304.5 ksi
ASTM D790
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.2 °C
180 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F