Abatron LiquidWood® Deep Penetrating Wood Consolidant

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Abatron
Trade Name LiquidWood®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron LiquidWood® Deep Penetrating Wood Consolidant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LiquidWood® is a deep penetrating wood consolidant that regenerates and waterproofs rotted, dried-out, or spongy wood. It restores structural strength and durability to wood fibers. With LiquidWood®, a piece of deteriorated wood that could crumble under finger pressure can be impregnated and restored to a rigid, durable, water and weather resistant wood superior to the original. The hardened mass can be sawed, planed, routed, carved, drilled, nailed, sanded, glued, and painted. LiquidWood® is also a primer for WoodEpox®. LiquidWood® is ideal for regenerating and waterproofing rotted, dried-out, or spongy window sills, thresholds, window and door frames, columns, stair steps, balustrades, floors, capitals, moldings, doors, shutters, indoor and outdoor furniture, archaeological and art restoration, boats, and millwork of all kinds. LiquidWood® has exceptional adhesion, structural strength, versatility, permanence, dimensional stability, and water resistance. LiquidWood® A and B are easy-to-use, are 100% reactive compounds, and contain no VOC's or noxious odors. Contents ? LiquidWood® consists of 2 clear, epoxy liquids: resin (A) and hardener (B). When A and B are mixed together in equal volumes, by simple stirring, a blend is formed with unique properties to impregnate and restore wood and other porous masses. Application ? Pour on brush on the wood where it penetrates the fibers and hardens into a water-resistant, distortion-free, high-strength mass in hours or minutes. 100% solids. 1/1 ratio. 30 minute pot life.
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Volatile Organic Compounds (VOC) Content 0.00 g/l
0.00 g/l
Mechanical Properties Metric English Comments
Hardness, Shore D 42
42
Tensile Strength at Break 10.1 MPa
1460 psi
Elongation at Break 84 %
84 %
Flexural Strength 6.21 MPa
900 psi
Compressive Strength 35.9 MPa
5210 psi
Processing Properties Metric English Comments
Pot Life 30 min
30 min