Abatron L060421-1 Heat-Resistant (-75~400°F) Non-Flammable Silicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Abatron
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron L060421-1 Heat-Resistant (-75~400°F) Non-Flammable Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
L060421-1 is a heat-resistant and non-flammable silicone rubber recommended as a potting compound for exceptional protection against thermal shock, vibration, moisture, ozone, dust, chemicals, and other environmental hazards. Properties: (1) Retains elastomeric properties at temperatures up to 400°F; (2) Chemical composition contains no solvents for ease of use on production lines; (3) Convenient 1:1 mix ratio be weight or volume for use in automatic dispensing or hand operations; (4) Low viscosity allows easy flow in and around complex parts; (5) Cures in deep sections or enclosed assemblies without exotherm and with low shrinkage.
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
Tensile Strength at Break 3.31 MPa
480 psi
Elongation at Break 60 %
60 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -59.4 °C
-75.0 °F
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 150 °C
0.250 hour

@Temperature 302 °F
60.0 min

@Temperature 100 °C
1.00 hour

@Temperature 212 °F
240 min

@Temperature 65.0 °C
4.00 hour

@Temperature 149 °F
2880 min

@Temperature 25.0 °C
48.0 hour

@Temperature 77.0 °F
Shelf Life 12.0 Month

@Temperature <=26.7 °C
12.0 Month

@Temperature <=80.0 °F
Descriptive Properties Value Comments
Color Opaque Gray