Material Notes:
AboWeld 8104-12 is a 2-part, 100% solids, liquid or filled polysulfide-epoxy. It is available in many colors. It is often used with sand and gravel to mix grouts for filling and resurfacing. It is primarily for strong adhesion on floors with heavy traffic.
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Mechanical Properties Metric English Comments
Hardness, Shore A 57 - 60
57 - 60
Tensile Strength at Break 1.38 - 1.52 MPa
200 - 220 psi
Elongation at Break 150 - 200 %
150 - 200 %
Processing Properties Metric English Comments
Cure Time 1440 - 4320 min
24.0 - 72.0 hour
(1-3 Days)
Pot Life 60 min
60 min
Descriptive Properties Value Comments
Color Many Colors
Parts by Weight (pbw) 1
Part B
2
Part A