AboGlass-1 is a combination of a clear resin compound and a clear hardener. It is a virtually colorless, clear liquid, 2-part, epoxy system for casting layers up to 2 or more inches, and for embedments. It is used on tabletops, counters, pictures, and artifacts. AboGlass-1 offers: (1) Virtually colorless, glass-like, transparency; (2) Low viscosity for pouring, wetting, and self-leveling; (3) superior hardness and abrasion resistance; (4) High impact resistance; (5) Outstanding water and weather resistance; (6) Machineable; (7) Superior tabletop resurfacer; (8) Can be applied in thick or thin layers. It offers the best recoat adhesion within the first 1-4 days. After this period, it should be sanded (or reprimed with the same Primkote 8006-1) if it is glossy and difficult to wet. It can also be used alone, in one or several coats, to protect metal surfaces from rust, to make a flat surface glossy, or to protect a color pattern.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
Density 1.05 g/cc
0.0381 lb/in³
Solids Content 100 %
100 %
Viscosity 1750 cP
1750 cP
Processing Properties Metric English Comments
Pot Life 25 min
25 min
Descriptive Properties Value Comments
Gloss High
Hardening Time (min) 40-50
Induction Period (min) 5 to 10