Abatron AboCoat 8508-3 Self-Leveling Epoxy Coating and Resurfacer

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Abatron
Trade Name AboCoat
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCoat 8508-3 Self-Leveling Epoxy Coating and Resurfacer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AboCoat 8508-3 is a self-leveling epoxy coating and resurfacer. It is used for heavy-duty protection and rebuilding of smooth, spalled, cracked, or pitted floors. It can be applied to concrete, masonry, wood, metal, glass, and composite surfaces. It is ideal for seamless floors in heavy-traffic areas and can be used with sand or grit to make a great anti-slip surface. Features: Contains no water or solvents; Can be applied in any thickness; Primer recommended; Available in standard and custom colors; 2-component (3:1 by volume); Virtually shrink-free. Benefits: Can be mixed with sand and gravel to level damaged areas; Excellent chemical and salt resistance; Superior wear resistance; Superior color retention.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 0.00 g/l
0.00 g/l
EPA method #24
Mechanical Properties Metric English Comments
Elongation at Break 7.6 %
7.6 %
ASTM-D638
Compressive Strength 124 MPa
18000 psi
ASTM-D695
Adhesive Bond Strength 13.01 MPa
1887 psi
ASTM-D4541
Coefficient of Friction 1.43
1.43
Slip resistance; ASTM-D1894
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
ASTM-D2485
Processing Properties Metric English Comments
Processing Temperature 15.6 - 29.4 °C
60.0 - 85.0 °F
Application Temperature
Cure Time 10080 - 30240 min

@Temperature 20.0 °C
168.0 - 504.0 hour

@Temperature 68.0 °F
(1-3 weeks)
Pot Life 50 min

@Temperature 24.0 °C
50 min

@Temperature 75.2 °F
100 g
Shelf Life >= 24.0 Month
>= 24.0 Month
Descriptive Properties Value Comments
Abrasive Resistance (g) 0.16
ASTM-D4060; CS 17/Load 1000/Cycles 1000
Hardening Time (min) 60-180
Hardness, pencil 3H
ASTM-D3363
Impact Resistance 5
ASTM-D4226