Material Notes:
AboCast 8503-3/AboCure 8503-3 is a general purpose, medium speed, colorless epoxy casting compound with low viscosity. It has a good balance of properties with a fairly fast hardening. Suggested Uses: Transparent Casting, Embedding, Encapsulation, Potting, and Bonding. Casting display or experimental models without the high shrinkage of acrylic or other resins. Precise reproduction of anatomical or scientific models. Embedding organic, geologic, or metallurgic specimens. Encapsulation of electric, radioactive, or delicate components. Preservation or repair of artistic and historical objects. High-performance transparent table tops.
Physical Properties Metric English Comments
Viscosity 800 cP
800 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
Tensile Strength at Break 54.5 MPa
7900 psi
Elongation at Break 16 %
16 %
Flexural Strength 71.0 MPa
10300 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 51.0 °C
124 °F
Deflection Temp at unknown load
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Pot Life 45 min

@Temperature 25.0 °C
45 min

@Temperature 77.0 °F
500 g
Descriptive Properties Value Comments
Hardening Time (min) 60-600
Parts by Weight (pbw) 100
AboCast
60
AboCure