Abatron AboCast 8-5/Abocure 8-5 Epoxy  (discontinued **)

Category Polymer , Thermoset , Epoxy
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 8-5/Abocure 8-5 Epoxy  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
2-part solvent-free dielectric epoxy casting compound.Processing: 100/80.5 ratio (pbw); Gel time, 100 g (3.5 oz.): 300 minutes; cures in 3 weeks at 25°C (77°F).Applications: solventless casting, adhesive, and coating.
Physical Properties Metric English Comments
Water Absorption 0.52 %
0.52 %
in 24 hours.
Viscosity Measurement 1000
1000
Mechanical Properties Metric English Comments
Hardness, Shore D 81
81
Tensile Strength, Ultimate 40.68 MPa
5900 psi
Elongation at Break 15 %
15 %
Flexural Strength 65.15 MPa
9449 psi
Electrical Properties Metric English Comments
Electrical Resistivity 8.00e+9 ohm-cm

@Temperature 93.3 °C
8.00e+9 ohm-cm

@Temperature 200 °F
8.00e+11 ohm-cm

@Temperature 65.6 °C
8.00e+11 ohm-cm

@Temperature 150 °F
2.00e+15 ohm-cm

@Temperature 25.0 °C
2.00e+15 ohm-cm

@Temperature 77.0 °F
Dielectric Constant 3.3

@Frequency 1e+6 Hz
3.3

@Frequency 1e+6 Hz
Dissipation Factor 0.016

@Frequency 1e+6 Hz
0.016

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F
Curing time: 3 weeks
Users viewing this material also viewed the following: