Abatron AboCast 7802-1/AboCure 50-11 Epoxy  (discontinued **)

Category Polymer , Thermoset , Epoxy
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 7802-1/AboCure 50-11 Epoxy  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Abatron, Inc. Low-viscosity, Light Amber color. Shelf life is 12+ months.Processing: 2/1 ratio. Pot life: 40-50 min. Lower viscosity and shorter pot life than Abocast 50-3/Abocure 8012-3.Applications: General-purpose casting, floor resurfacing, and coating.
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Typical value for Abatron "VR" Epoxies.
Tensile Strength, Ultimate 55.0 MPa
7980 psi
Typical value for Abatron "VR" Epoxies.
Compressive Yield Strength 62.0 MPa
8990 psi
Typical value for Abatron "VR" Epoxies.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 75.0 °C
167 °F
70-80°C (160-175°F) Heat distortion temperature.