Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Abatron AboCast 10-5/AboCure 50-17 Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy, Cast, Unreinforced
Manufacturer Abatron
Trade Name AboCast
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 10-5/AboCure 50-17 Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AboCast 10-5 is a filled, high-viscosity epoxy resin. It is blended with AboCure 50-17 to make a structural adhesive and casting compound for the optic and electric industry. AboCure 50-17 is a high-temperature, chemical resistant, and high-modulus liquid converter. AboCast 10-5/AboCure 50-17 has the highest modulus, hardness, heat resistance, and chemical resistance in the AboCast 10-5 series. It allow the largest castings, over 5 gallons per pouring. This system has far higher resistance to strong solvents and other chemical agents than the other compounds. This blend's main advantages are: it has low-viscosity and is very slow, very hard, high heat resistant, chemical resistant, and is used for large castings. It also is dielectric and offers good adhesion, virtually no shrinkage, and high resistance to alkalis, diluted acids, water, many solvents, and outdoors.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 °C
320 °F
Processing Properties Metric English Comments
Pot Life 360 - 480 min

@Temperature 25.0 °C
360 - 480 min

@Temperature 77.0 °F
100 g
Descriptive Properties Value Comments
Color Green
Hardening Time (min) 36 to 60
25°C
Parts by Weight (pbw) 100
AboCast 10-5
13
AboCure 50-17
Viscosity Fluid
Users viewing this material also viewed the following: