Abatron 7908-2A/5012B Filled Potting Compound  (discontinued **)

Category Polymer , Adhesive , Thermoset
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron 7908-2A/5012B Filled Potting Compound  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Green or colors dielectric heat sink 57% filled. 100/5.6 ratioInformation provided by Abatron.
Physical Properties Metric English Comments
Filler Content 57 %
57 %
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Processing Properties Metric English Comments
Pot Life >= 40 min
>= 40 min
Descriptive Properties Value Comments
Color Green
Viscosity High