Abatron 7907-2A/5017B Filled Potting Compound  (discontinued **)

Category Polymer , Adhesive , Thermoset
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron 7907-2A/5017B Filled Potting Compound  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tan or color dielectric structural casting adhesive. 100/15 ratio. High functional heat cure.Information provided by Abatron.
Physical Properties Metric English Comments
Filler Content 53 %
53 %
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Processing Properties Metric English Comments
Pot Life >= 400 min
>= 400 min
Descriptive Properties Value Comments
Color Tan
Viscosity Medium