Material Notes:
Machinable room temperature casting/tooling epoxy system. 100/8 ratio.Information provided by Abatron.
Physical Properties Metric English Comments
Filler Content 55.6 %
55.6 %
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
Processing Properties Metric English Comments
Pot Life >= 40 min
>= 40 min
Descriptive Properties Value Comments
Color Gray
Viscosity Medium