Abatron 7703-2A/5017B Filled Potting Compound  (discontinued **)

Category Polymer , Adhesive , Thermoset
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron 7703-2A/5017B Filled Potting Compound  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tan and colors dielectric heat sink paste with 65% alumina filler. 100/8 ratio.Information provided by Abatron.
Physical Properties Metric English Comments
Filler Content 65 %
65 %
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 °C
320 °F
Processing Properties Metric English Comments
Pot Life >= 360 min
>= 360 min
Descriptive Properties Value Comments
Color Tan
Viscosity High