Abatron 7703-2A/5012B Filled Potting Compound  (discontinued **)

Category Polymer , Adhesive , Thermoset
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron 7703-2A/5012B Filled Potting Compound  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heat sink castable dielectric paste. 67% alumina filler. 100/4 ratio.Information provided by Abatron.
Physical Properties Metric English Comments
Filler Content 67.3 %
67.3 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 115 °C
239 °F
Processing Properties Metric English Comments
Pot Life >= 40 min
>= 40 min
Descriptive Properties Value Comments
Color Neutral
Viscosity High