Abatron 223 A/B Filled Potting Compound  (discontinued **)

Category Polymer , Adhesive , Thermoset
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron 223 A/B Filled Potting Compound  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dielectric structural casting adhesive for potting and embedding white and colors. 2/1 ratio.Information provided by Abatron.
Physical Properties Metric English Comments
Filler Content 50 %
50 %
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
Processing Properties Metric English Comments
Pot Life >= 40 min
>= 40 min
Descriptive Properties Value Comments
Color White
Viscosity High