Abatron 105A/50-12B Filled Potting Compound  (discontinued **)

Category Polymer , Adhesive , Thermoset
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron 105A/50-12B Filled Potting Compound  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Green dielectric structural casting adhesive for metal, glass, ceramics, and etc. 6.5 ratio; chemical resistance 100.Information provided by Abatron.
Physical Properties Metric English Comments
Filler Content 50.2 %
50.2 %
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Processing Properties Metric English Comments
Pot Life >= 40 min
>= 40 min
Descriptive Properties Value Comments
Color Green
Viscosity High