Melt flow index may be specified.
Physical Properties Metric English Comments
Specific Gravity 0.930 - 0.945 g/cc
0.930 - 0.945 g/cc
ASTM D792
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Melt Flow 2.0 - 120 g/10 min

@Load 5.00 kg,
Temperature 190 °C
2.0 - 120 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 20.7 MPa
3000 psi
ASTM D638
Flexural Modulus 0.724 GPa
105 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256