Aaron Industries AVPE LD 300-1 MELT 20 Virgin Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Aaron Industries Corporation
Trade Name AVPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AVPE LD 300-1 MELT 20 Virgin Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A natural, high flow Low Density Polyethylene resin, specifically designed for high speed injection molding applications.
Physical Properties Metric English Comments
Specific Gravity 0.925 g/cc
0.925 g/cc
ASTM D792
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Melt Flow 20 g/10 min

@Load 5.00 kg,
Temperature 190 °C
20 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 10.3 MPa
1500 psi
ASTM D638
Tensile Strength, Yield 8.96 MPa
1300 psi
ASTM D638
Izod Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.8 °C
163 °F
ASTM D648