Aaron Industries AAROPRENE® MFN 6001 Mineral Filled Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Aaron Industries Corporation
Trade Name AAROPRENE® MFN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AAROPRENE® MFN 6001 Mineral Filled Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AAROPRENE® GFN &G/MFN 6000 Series Reinforced CompoundsColor may be specified.
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 82.7 MPa
12000 psi
ASTM D638
Flexural Modulus 5.24 GPa
760 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256