Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aaron Industries AAROPRENE® GFN 6033 Glass Filled Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Aaron Industries Corporation
Trade Name AAROPRENE® GFN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AAROPRENE® GFN 6033 Glass Filled Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AAROPRENE® GFN &G/MFN 6000 Series Reinforced CompoundsColor may be specified.
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 162 MPa
23500 psi
ASTM D638
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 1.12 J/cm
2.10 ft-lb/in
ASTM D256