Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aaron Industries AAROLENE® ARPP H 200-1 Polypropylene Compounded Resin

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Aaron Industries Corporation
Trade Name AAROLENE® ARPP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AAROLENE® ARPP H 200-1 Polypropylene Compounded Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AAROLENE® ARPP 200 Series Polypropylene Compounded ResinColor may be specified. Melt Flow Index may be specified.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Linear Mold Shrinkage 0.022 cm/cm
0.022 in/in
ASTM D955
Melt Flow 4.0 - 30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 - 30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 28.3 MPa
4100 psi
ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Izod Impact, Notched 0.427 - 0.534 J/cm
0.800 - 1.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 128 °C
262 °F
ASTM D648