Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aardvark Polymers AARTEL® 100 D/S Rotational Molding Resin

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer Gehrig & Associates
Trade Name AARTEL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aardvark Polymers AARTEL® 100 D/S Rotational Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Aartel 100SD is a new conductive grade developed to dissipate electricity in fuel handling systems. Aartel 100SD maintains all o the excellent properties of our general purpose acetal, has a volume resistivity of 5E00 ohm-m, and has an improved resistance to hot diesel fuels.Information provided by Gehrig & Associates
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
Linear Mold Shrinkage 0.019 cm/cm
0.019 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.020 cm/cm
0.020 in/in
ISO 294-4
Melt Flow 1.38 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.38 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 49.0 MPa
7110 psi
(50mm/min); ISO 527-2/1A
Elongation at Yield 6.2 %
6.2 %
(50mm/min); ISO 527-2/1A
Tensile Modulus 2.45 GPa
355 ksi
(1mm/min); ISO 527-2/1A
Flexural Modulus 2.40 GPa
348 ksi
ISO 178
Izod Impact, Notched (ISO) 4.20 kJ/m²

@Temperature 23.0 °C
2.00 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Charpy Impact, Notched 0.440 J/cm²

@Temperature 23.0 °C
2.09 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1e
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
(10°C/min); ISO 11357-1,2,3
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ISO 75-1/-2