Material Notes:
A white, crystalline powder.Information provided by ATI Wah ChangTypical Analysis: On Zr metal basis
Physical Properties Metric English Comments
Molecular Weight 267.23 g/mol
267.23 g/mol
Component Elements Properties Metric English Comments
Chlorine, Cl <= 0.010 %
<= 0.010 %
Hafnium, Hf <= 0.010 %
<= 0.010 %
Silicon, Si <= 0.010 %
<= 0.010 %
Descriptive Properties Value Comments
Nominal Purity % 99.9