ATI Allvac® Vasco® 455 Specialty Steel, Heat Treatment: 829°C (1525°F) + Age

Category Metal , Ferrous Metal , Stainless Steel , T 400 Series Stainless Steel
Manufacturer ATI Allvac
Trade Name Vasco®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® Vasco® 455 Specialty Steel, Heat Treatment: 829°C (1525°F) + Age.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Allvac.Applications: High-strength aircraft components including fasteners, bolts, pins, pressure vessels, gears, shafts.
Physical Properties Metric English Comments
Density 7.83 g/cc
0.283 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 389
389
Estimated from Rockwell C value for Brinell test with 3000 kg load/10 mm diameter ball
Hardness, Knoop 425
425
Estimated from Rockwell C value.
Hardness, Rockwell C 42
42
Hardness, Vickers 407
407
Estimated from Rockwell C value.
Tensile Strength, Ultimate 1517 MPa
220000 psi
Tensile Strength, Yield 1413 MPa

@Strain 0.200 %
204900 psi

@Strain 0.200 %
Elongation at Break >= 10 %
>= 10 %
Reduction of Area >= 40 %
>= 40 %
Component Elements Properties Metric English Comments
Carbon, C 0.030 %
0.030 %
Chromium, Cr 11.8 %
11.8 %
Copper, Cu 2.0 %
2.0 %
Iron, Fe 75 %
75 %
as balance
Manganese, Mn 0.25 %
0.25 %
Molybdenum, Mo 0.25 %
0.25 %
Nickel, Ni 8.5 %
8.5 %
Niobium, Nb (Columbium, Cb) 0.30 %
0.30 %
Phosphorous, P 0.020 %
0.020 %
Silicon, Si 0.25 %
0.25 %
Sulfur, S 0.015 %
0.015 %
Titanium, Ti 1.1 %
1.1 %