ATI Allvac® Vasco® 410/403 Specialty Steel, Heat Treatment: 927°C (1700°F) Anneal

Category Metal , Ferrous Metal , Stainless Steel , T 400 Series Stainless Steel
Manufacturer ATI Allvac
Trade Name Vasco®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® Vasco® 410/403 Specialty Steel, Heat Treatment: 927°C (1700°F) Anneal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Allvac.Applications: Compressor blades, turbine parts.
Physical Properties Metric English Comments
Density 7.70 g/cc
0.278 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 90
90
Tensile Strength, Ultimate 690 MPa
100000 psi
Tensile Strength, Yield 621 MPa

@Strain 0.200 %
90100 psi

@Strain 0.200 %
Elongation at Break 22 %
22 %
Reduction of Area 65 %
65 %
Component Elements Properties Metric English Comments
Carbon, C 0.15 %
0.15 %
Chromium, Cr 12 %
12 %
Iron, Fe 87 %
87 %
as balance
Manganese, Mn 0.50 %
0.50 %
Phosphorous, P 0.020 %
0.020 %
Silicon, Si 0.50 %
0.50 %
Sulfur, S 0.010 %
0.010 %
Users viewing this material also viewed the following: