Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ATI Allvac® Nickelvac® 80 A UNS N07080 Nickel Superalloy

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer ATI Allvac
Trade Name Nickelvac®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® Nickelvac® 80 A UNS N07080 Nickel Superalloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Uses: Components for gas turbine engines, exhaust valve stock for internal combustion engines, high temperature bolts & fasteners.Property values are for samples in the metallurgical condition: 1700°F age.Information provided by Allvac, An Allegheny Teledyne Company.
Physical Properties Metric English Comments
Density 8.16 g/cc
0.295 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 39
39
Tensile Strength, Ultimate 1310 MPa
190000 psi
Tensile Strength, Yield 965 MPa

@Strain 0.200 %
140000 psi

@Strain 0.200 %
Elongation at Break 21 %
21 %
Reduction of Area 25 %
25 %
Component Elements Properties Metric English Comments
Aluminum, Al 1.4 %
1.4 %
Boron, B 0.0020 %
0.0020 %
Carbon, C 0.050 %
0.050 %
Chromium, Cr 19.5 %
19.5 %
Cobalt, Co 1.0 %
1.0 %
Copper, Cu 0.10 %
0.10 %
Iron, Fe 1.5 %
1.5 %
Manganese, Mn 0.50 %
0.50 %
Nickel, Ni 70 %
70 %
Phosphorous, P 0.020 %
0.020 %
Silicon, Si 0.50 %
0.50 %
Sulfur, S 0.0080 %
0.0080 %
Titanium, Ti 2.38 %
2.38 %
Users viewing this material also viewed the following: