Material Notes:
Uses: Weld wire, woven wire mesh belts, rod for heat treat baskets, heat treat fixtures.Property values are for samples in the metallurgical condition: 1950°C anneal.Information provided by Allvac, An Allegheny Teledyne Company.
Physical Properties Metric English Comments
Density 8.05 g/cc
0.291 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 65
65
Tensile Strength, Ultimate 621 MPa
90100 psi
Tensile Strength, Yield 207 MPa

@Strain 0.200 %
30000 psi

@Strain 0.200 %
Elongation at Break 55 %
55 %
Reduction of Area 65 %
65 %
Component Elements Properties Metric English Comments
Aluminum, Al 1.3 %
1.3 %
Carbon, C 0.050 %
0.050 %
Chromium, Cr 23 %
23 %
Copper, Cu 0.50 %
0.50 %
Iron, Fe 14 %
14 %
as balance
Manganese, Mn 0.50 %
0.50 %
Nickel, Ni 60.5 %
60.5 %
Silicon, Si 0.20 %
0.20 %
Sulfur, S 0.0080 %
0.0080 %