ATI Allvac® 8-1-1 Titanium Alloy, Heat Treatment: 982°C (1800°F) + Age

Category Metal , Nonferrous Metal , Titanium Alloy , Alpha/Near Alpha Titanium Alloy
Manufacturer ATI Allvac
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® 8-1-1 Titanium Alloy, Heat Treatment: 982°C (1800°F) + Age.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Allvac.Applications: Fan & compressor blades, discs, spacers, seals, rings. Excellent creep resistance. Standard, rotor/premium grades.
Physical Properties Metric English Comments
Density 4.31 g/cc
0.156 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 326
326
Estimated from Rockwell C value for Brinell test with 3000 kg load/10 mm diameter ball
Hardness, Knoop 354
354
Estimated from Rockwell C value.
Hardness, Rockwell C 35
35
Hardness, Vickers 341
341
Estimated from Rockwell C value.
Tensile Strength, Ultimate 1035 MPa
150100 psi
Tensile Strength, Yield 966 MPa

@Strain 0.200 %
140000 psi

@Strain 0.200 %
Elongation at Break 15 %
15 %
Reduction of Area 40 %
40 %
Component Elements Properties Metric English Comments
Aluminum, Al 8.0 %
8.0 %
Carbon, C 0.030 %
0.030 %
Hydrogen, H <= 0.015 %
<= 0.015 %
Iron, Fe 0.13 %
0.13 %
Molybdenum, Mo 1.0 %
1.0 %
Nitrogen, N 0.010 %
0.010 %
Phosphorous, P 0.20 %
0.20 %
Titanium, Ti 90 %
90 %
as balance
Vanadium, V 1.0 %
1.0 %