ATI Allvac® 6-2-4-2-Si UNS R54620 modified Titanium Alloy

Category Metal , Nonferrous Metal , Titanium Alloy
Manufacturer ATI Allvac
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® 6-2-4-2-Si UNS R54620 modified Titanium Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Uses: High performance valves for internal combustion engines. Aerospace and commercial grades.Property values are for samples in the metallurgical condition: 1800°F anneal.Information provided by Allvac, An Allegheny Teledyne Company.
Physical Properties Metric English Comments
Density 4.54 g/cc
0.164 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 28
28
Tensile Strength, Ultimate 1035 MPa
150100 psi
Tensile Strength, Yield 966 MPa

@Strain 0.200 %
140000 psi

@Strain 0.200 %
Elongation at Break 15 %
15 %
Reduction of Area 30 %
30 %
Component Elements Properties Metric English Comments
Aluminum, Al 6.0 %
6.0 %
Carbon, C <= 0.10 %
<= 0.10 %
Hydrogen, H <= 0.015 %
<= 0.015 %
Iron, Fe 0.050 %
0.050 %
Molybdenum, Mo 2.0 %
2.0 %
Nitrogen, N 0.040 %
0.040 %
Oxygen, O 0.20 %
0.20 %
Silicon, Si 0.12 %
0.12 %
Tin, Sn 2.0 %
2.0 %
Titanium, Ti 85 %
85 %
as balance
Zirconium, Zr 4.0 %
4.0 %