ATI Allvac® 40, Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal

Category Metal , Nonferrous Metal , Titanium Alloy , Unalloyed/Modified Titanium
Manufacturer ATI Allvac
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® 40, Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Allvac.Applications: Airframe components, cryogenic vessels, heat exchangers, CPI equipment, condenser tubing, pickling baskets.
Physical Properties Metric English Comments
Density 4.51 g/cc
0.163 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 80
80
Tensile Strength, Ultimate 345 MPa
50000 psi
Tensile Strength, Yield 276 MPa

@Strain 0.200 %
40000 psi

@Strain 0.200 %
Elongation at Break 20 %
20 %
Reduction of Area 30 %
30 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.10 %
<= 0.10 %
Hydrogen, H <= 0.015 %
<= 0.015 %
Iron, Fe <= 0.30 %
<= 0.30 %
Nitrogen, N <= 0.030 %
<= 0.030 %
Oxygen, O <= 0.25 %
<= 0.25 %
Titanium, Ti 99 %
99 %
as balance