ATI Allegheny Ludlum D2 Tool Steel, UNS T30402

Category Metal , Ferrous Metal , Tool Steel
Manufacturer ATI Allegheny Ludlum
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allegheny Ludlum D2 Tool Steel, UNS T30402.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
An air hardening grade with good nondeforming properties. Widely used in applications requiring high abrasion resistance and high compressive strength, such as blanking, forming and stamping dies, forming and scanning rolls, slitters and gages.Information provided by Allegheny Ludlum
Component Elements Properties Metric English Comments
Carbon, C 1.5 %
1.5 %
Chromium, Cr 12 %
12 %
Iron, Fe 85 %
85 %
as balance
Molybdenum, Mo 1.0 %
1.0 %
Vanadium, V 0.80 %
0.80 %