ATI Allegheny Ludlum AL 17-7™ High Strength Stainless Steel, UNS S17700

Category Metal , Ferrous Metal , Stainless Steel , Precipitation Hardening Stainless
Manufacturer ATI Allegheny Ludlum
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allegheny Ludlum AL 17-7™ High Strength Stainless Steel, UNS S17700.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Property data below is typical of annealed samples. Available in sheet and strip. For use in high-strength springs, bellows, and aerospace applications.Information provided by Allegheny Ludlum
Physical Properties Metric English Comments
Density 7.81 g/cc
0.282 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 85
85
Tensile Strength, Ultimate 830 MPa
120000 psi
Tensile Strength, Yield 345 MPa

@Strain 0.200 %
50000 psi

@Strain 0.200 %
Elongation at Break 35 %
35 %
Component Elements Properties Metric English Comments
Aluminum, Al 1.1 %
1.1 %
Chromium, Cr 17 %
17 %
Iron, Fe 74.9 %
74.9 %
as balance
Nickel, Ni 7.0 %
7.0 %