ATG s.r.l. CR Polychloroprene

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer ATG s.r.l.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATG s.r.l. CR Polychloroprene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 25 - 90
25 - 90
Tensile Strength, Ultimate 7.00 - 24.0 MPa
1020 - 3480 psi
Elongation at Break 100 - 800 %
100 - 800 %
Rebound 20 - 50 %
20 - 50 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Descriptive Properties Value Comments
Abrasion Resistance high
Chemical Resistance to Animal and Vegetable Oils and Greases medium
Chemical Resistance to Aromatic Hydrocarbons none
Chemical Resistance to Chloride Solvents none
Chemical Resistance to Distilled Water medium
Chemical Resistance to Ketones low
Chemical Resistance to Maximum Concentrated Alkalis (at 50°C) high
Chemical Resistance to Medium-High Concentrated Acids (at 50°C) low
Chemical Resistance to Mineral Oils and Aliphatic Hydrocarbons medium
Compression set at 100°C medium
Impermeability at gas (Oxygen and Nitrogen) high
Resistance to Flame high
Resistance to Heat Aging low
Resistance to Low Temperatures low
Resistance to Ozone and Weathering high
Tear Strength high